<span>Vertical ZnO 3D nanostructures were synthesized on Au covered c-plane GaN epilayer film on sapphire substrate by chemical vapor deposition method. The growth was conducted in a horizontal tube furnace with 1" diameter quartz tube. High purity ZnO powder and </span><span>oxygen were used as the precursors. The growth was carried out for 1 hr at 900 C. The growth direction was polar. The image shows the 20 degree tilted view of the nanostructures. The image was taken at the Swagelok Center for Surface Material Analysis (SCSAM) at CWRU.</span>